Coil, Sheet & Plates
Grade :- 304, 304L, 304H, 316, 316L, 316LN, 316Ti, 309, 310S, 317L, 321, 347, 409, 410, 420, 430, 446 & 202
Sheet Finishing :- 2B, 2D, HR, CR, BA (No. 8), Satin (Reliable Pipes and Tubes Ltd. with Plastic Coated)
Sheet & Plate in Form of :- Coils, Foils, Shim Sheet, Perforated Sheet,Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) & Angle, Channel, Tray Etc.
Other Services :- Heat Treatment, Annealing, Pickling, Polish, Electroplating, Anodising, Rolling, Cutting, Bending, Forging, Minor Fabrication Etc.
Test Certificate :- Manufacturer Test Certificate / Laboratory Test Certificate from Govt. Approved Lab. & Under Third Party Inspection.
Size :- Thickness: 0.1 mm to 48 mm, Width: 1000 mm to 2500 mm, Length: 2000 mm to Coil.
We offer highly customized steel plates, carbon steel coils, carbon steel sheets to our customers and provide them in different grades like, low carbon grade, high carbon grade and straight grade that meets the specific requirements of the clients. Stainless steel is the most ideal material for plates and the only material that requires almost no maintenance. Stainless steel is the least expensive material and they never chip or corrode and hence last forever.
Sheet Finishing :- 2B, 2D, HR, CR, BA (No. 8), Satin (Reliable Pipes and Tubes Ltd. with Plastic Coated)
Sheet & Plate in Form of :- Coils, Foils, Shim Sheet, Perforated Sheet,Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) & Angle, Channel, Tray Etc.
Other Services :- Heat Treatment, Annealing, Pickling, Polish, Electroplating, Anodising, Rolling, Cutting, Bending, Forging, Minor Fabrication Etc.
Test Certificate :- Manufacturer Test Certificate / Laboratory Test Certificate from Govt. Approved Lab. & Under Third Party Inspection.
Size :- Thickness: 0.1 mm to 48 mm, Width: 1000 mm to 2500 mm, Length: 2000 mm to Coil.
We offer highly customized steel plates, carbon steel coils, carbon steel sheets to our customers and provide them in different grades like, low carbon grade, high carbon grade and straight grade that meets the specific requirements of the clients. Stainless steel is the most ideal material for plates and the only material that requires almost no maintenance. Stainless steel is the least expensive material and they never chip or corrode and hence last forever.
User Industries:
Chemicals, Fats, & Fertilizers, Sugar Mills & Distilleries, Cement Industries, Ship Builders, Paper Industries, Pumps, Petrochemicals, Oil & Natural Gas Organization in terms of the specific materials, Technology, Finance & Personal.
Chemical Composition of Sheets/ Plates
ASTM | Grade | C max | Mn max | P max | S max | Si max | Ni | Cr | Mo | Others |
A240 | 304 | |||||||||
0.08 | 200 | 0.045 | 0.03 | 0.75 | 8.00-11.0 | 18.0-20.0 | ||||
304L | 0.03 | 200 | 0.045 | 0.03 | 0.75 | 8.00-11.0 | 18.0-20.0 | |||
310S | 0.08 | 200 | 0.045 | 0.03 | 1.5 | 19.0-22.0 | 24.0-26.0 | |||
316 | 0.08 | 200 | 0.045 | 0.03 | 0.75 | 10.0-14.0 | 16.0-18.0 | 2.00-3.00 | ||
316L | 0.03 | 200 | 0.045 | 0.03 | 0.75 | 10.1-14.0 | 16.0-18.0 | 2.00-3.00 | ||
317L | 0.03 | 200 | 0.045 | 0.03 | 0.75 | 11.0-15.0 | 18.0-20.0 | 3.00-4.00 | ||
321 | 0.08 | 200 | 0.045 | 0.03 | 0.75 | 9.00-12.0 | 17.0-20.0 | 5C<Ti<0.70% | ||
347 | 0.08 | 200 | 0.045 | 0.03 | 0.75 | 9.00-13.0 | 17.0-20.0 | 10C<Cb+Ta<1.10% |
Mechanical Requirements | Hardness | |||||
ASTM | Grade | Tensile Strength Apa (ksi) min | Yield Strength Mpa (ksi)min | Elongation min% | ||
Brinel max HB | Rockwell max HRB | |||||
A240 | 304 | 205(30) | 205(30) | 40 | 202 | 92 |
304L | 170(25) | 170(25) | 40 | 183 | 92 | |
310S | 205(25) | 205(25) | 40 | 217 | 88 | |
316 | 205(30) | 205(30) | 40 | 217 | 95 | |
316L | 170(25) | 170(25) | 40 | 217 | 95 | |
317L | 170(25) | 170(25) | 40 | 217 | 95 | |
321 | 205(30) | 205(30) | 40 | 217 | 95 | |
347 | 205(30) | 205(30) | 40 | 183 | 92 |
Carbon Steel
Reliable supplies heavy plates, alloy steel coils, carbon steel coils, alloy steel sheets, hot rolled coils.
Both steel plate and hot rolled coils satisfy the more important needs from a technological and dimensional point of view.
Both steel plate and hot rolled coils satisfy the more important needs from a technological and dimensional point of view.
Plate |
Thickness : to a maximum of 200 mm; Width : from 1250 mm to 2500 mm. |
Coil |
Thickness : to a maximum of 20 mm; Width : up to a maximum 2000 mm |
Chemical Composition of Sheets/ Plates
ASTM | Grade | C max | Mn max | P max | S max | Si max | Ni | Cr | Mo | Others |
A 515 | 60 | 0.27 | 0.9 | 0.04 | 0.04 | 0.15.04 | ||||
70 | 0.33 | 1.2 | 0.04 | 0.04 | 0.15-0.40 | |||||
A 516 | 60 | 0.23 | 0.85-1.20 | 0.04 | 0.04 | 0.15-0.40 | ||||
70 | 0.28 | 0.85-1.20 | 0.04 | 0.4 | 0.15-0.40 | |||||
A 537 | Class 1 | 0.02 | 0.70-1.35 | 0.04 | 0.04 | 0.15-0.40 | 0.25max | 0.80 max | 0.35max | |
Class 2 | 0.24 | 0.70-1.35 | 0.04 | 0.04 | 0.15-0.40 | 0.25 max | 0.80 max | 0.35max |
Mechanical Requirements | Hardness | |||||
ASTM | Grade | Tensile Strength Apa (ksi) min | Yield Strength Mpa (ksi)min | Elongation min% | Brinel max HB | Rockwell max HRB |
A 515 | 60 | 415-550/(60-80) | 220(32) | 25 | _ | _ |
70 | 485-620/(70-90) | 260(38) | 21 | _ | _ | |
A 516 | 60 | 415-550/(60-80) | 220(32) | 25 | _ | _ |
70 | 485-620/(70-90) | 260(38) | 21 | _ | _ | |
A 537 | Class 1 | 485-620/(70-90) | 345(50) | 22 | _ | _ |
Class 2 | 550690/(80-100) | 415-60 | 22 | _ | _ |
Alloy Steel Plates SA 387
Chromoly is an abbreviation for "chromium-molybdenum steel". Chromoly is an alloy used to produce tubing for bicycle frames and race-car roll cages. It is not as lightweight as some steel alloys, but has the advantages of high tensile strength and malleability. It is also easily welded and is considerably stronger and more durable than standard (1020) steel tubing.
Chemical Composition of Sheets/ Plates | ||||||||||
ASTM | Grade | C max | Mn max | P max | S max | Si max | Ni | Cr | Mo | Others |
A387 Class 1 Class 2 | 5 | 0.15 | 0.30-0.60 | 0.04 | 0.03 | 0.5 | 4.00-6.00 | 0.45-0.65 | ||
9 | 0.15 | 0.30-3.60 | 0.03 | 0.3 | 1 | 8.00-10.0 | 0.90-1.10 | |||
11 | 0.04-0.17 | 0.40-0.65 | 0.04 | 0.04 | 0.50-0.80 | 1.00-1.50 | 0.45-0.65 | |||
12 | 0.04-0.17 | 0.40-0.65 | 0.04 | 0.04 | 0.15-0.40 | 0.80-1.15 | 0.45-0.60 | |||
22 | 0.05-0.17 | 0.30-0.60 | 0.04 | 0.035 | 0.5 | 2.00-2.50 | 0.90-1.10 |
Mechanical Requirements | Hardness | |||||||
ASTM | Grade | Tensile Strength Apa (ksi) min | Yield Strength Mpa (ksi)min | Elongation min% | Brinel max HB | Rockwell max HRB | ||
Class 1 | Class 2 | Class1 | Class2 | |||||
A387 Class 1 Class 2 | 5 | 415-585 | 515-690 | 205 | 310 | 18 | 202 | 92 |
9 | 415-585 | 515-690 | 205 | 310 | 18 | 217 | 95 | |
11 | 415-585 | 515-690 | 240 | 310 | 22 | 217 | 95 | |
12 | 380-550 | 450-585 | 230 | 275 | 22 | 217 | 95 | |
22 | 415-585 | 515-690 | 205 | 310 | 18 | 201 | 92 |